• cooltrainer_frank@lemmy.world
    link
    fedilink
    arrow-up
    1
    ·
    2 years ago

    Yup, the lab could tell a difference! Shiney side (so mill roller facing, as opposed to the dull side which faces the other layer of aluminum) was marginally more reflective, but I believe (and a former coworker also remembered it as) it was less than a tenth of a percent (<0.1% for the visual folks)

    Anyone who says it affects cooking time or something is mistaken, I’d wager.

    • evasive_chimpanzee@lemmy.world
      link
      fedilink
      arrow-up
      1
      ·
      2 years ago

      Any info on surface roughness? I’m thinking shiny side would be smoother and therefore less sticky, though I don’t know how much the passivation layer would affect it. Probably no where close to making a difference at the end of the day, but I’m curious.

      • cooltrainer_frank@lemmy.world
        link
        fedilink
        arrow-up
        1
        ·
        2 years ago

        It was a fair few years ago, but yeah, the oxidation on it will be so much smoother than the delta in surface roughness that I doubt it’d make much difference. Lemme reach out to a metallurgist from there and see what he thinks!